Hits:
Indexed by:会议论文
Date of Publication:2010-06-26
Included Journals:EI、CPCI-S、Scopus
Volume:675-677
Page Number:917-920
Key Words:thermal stress analysis; First Wall; ITER; reduced activation ferritic martensitic
Abstract:The temperature and strain distributions of the mockup composed of Cu-alloy with distinct structural material (SS316L and China Low Activation martensitic steel (CLAM)) were calculated and analyzed, based on a high heat flux (HHF) test recently reported with heat flux of 3.2MW/m(2). The calculated temperature and strain results in the first wall (FW), in which SS316L is as the structural material, showed good agreement with HI-IF test. By substituting CLAM steel for SS316L the contrast analysis indicates that the thermo-mechanical property for CLAM steel is better than that of SS316 at the same condition. Furthermore, the temperature and strain distributions of the FW were calculated under the condition of normal ITER operation: the surface heat flux is about 0.5MW/m(2) and volumetric heating due to neutron radiation is on the order of 15-20 MW/m(2).