location: Current position: Home >> Scientific Research >> Paper Publications

High Temperature Oxidation and Wear Behaviors of Ti-V-Cr Fireproof Titanium Alloy

Hits:

Indexed by:期刊论文

Date of Publication:2017-06-01

Journal:METALS

Included Journals:SCIE、Scopus

Volume:7

Issue:6

ISSN No.:2075-4701

Key Words:titanium alloy; fireproof; oxidation; high temperature wear; mechanism

Abstract:The high temperature oxidation and wear behaviors of Ti-35V-15Cr-0.3Si-0.1C fireproof titanium alloy were examined at 873 and 1073 K. The oxidation weight gain after oxidation at 1073 K for 100 h was significantly larger than that at 873 K. Based on the analyses of the oxidation reaction index and oxide layer, the oxidation process at 1073 K was mainly controlled by oxidation reaction at the interface between the substrate and oxide layer. Dry sliding wear tests were performed on a pin-on-disk tester in air conditions. The friction coefficient was smaller at 1073 K than that at 873 K, while the volume wear rate at 1073 K was larger due to formation of amount of oxides on the worn surface. When the wearing temperature increased from 873 to 1073 K, the wear mechanism underwent a transition from a combination of abrasive wear and oxidative wear to only oxidative wear.

Pre One:显微组织对医用TC4钛合金U型钉缩口的影响

Next One:CrMoWV钢的应力松弛行为及其预测