Analyze on rupture HP40Nb steel tubes from hydrogen production reformer furnace of petroleum company

点击次数:

论文类型:期刊论文

发表时间:2013-12-01

发表刊物:Huagong Xuebao/CIESC Journal

收录刊物:EI、PKU、ISTIC、Scopus

卷号:64

期号:SUPPL.1

页面范围:159-164

ISSN号:04381157

摘要:Hydrogen production reformer furnace tubes made of cast austenitic alloy steels serve in the temperature range of 1073-1173 K and pressure around 3-4 MPa. Though the design life is about 100000 h, premature failures within 3-8 years are more common, mainly caused by premature creep induced by overheating. The cast tube material undergoes microstructural changes with service exposure and as a consequence, degradation in strength. The methods of macro inspection, chemical analysis, microstructure, scanning electron microscope and mechanical properties testing were used to analyze on the rupture HP40Nb steel tubes from a hydrogen production reformer furnace of one petroleum company when they were used only 18 h during the test run.The rupture life was very short and needed to find the reason, in case the similar incidents. The results show that the reason of failure for the furnace tubes is high temperature creep rupture and over temperature seriously is the direct reason. ? All Rights Reserved.