location: Current position: Home >> Scientific Research >> Paper Publications

Composition, Microstructure, Phase Constitution and Fundamental Physicochemical Properties of Low-Melting-Point Multi-Component Eutectic Alloys

Hits:

Indexed by:期刊论文

Date of Publication:2017-02-01

Journal:JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY

Included Journals:SCIE、EI

Volume:33

Issue:2

Page Number:131-154

ISSN No.:1005-0302

Key Words:Multicomponent alloys; Eutectic alloy; Microstructure; Physicochemical properties

Abstract:Low-melting-point alloys have an extensive applications in the fields of materials processing, phase change energy storage, electronic and electrical automatic control, continuous casting simulation, welding, etc. Specifically, the eutectic compositions make up a large number of low-melting-point alloys that are exploited because of their desirable features like single melting peaks, excellent operational reliability, and casting fluidity. However, the fundamental physicochemical properties from the current available literature on low-melting-point multi-component eutectic alloys (LMP-MCEAs) are rather rare and lowly accurate, including the exact melting temperatures and compositions, constituent phases, microstructures and morphologies, melting enthalpies, specific heats, densities, and so on. This lack of information seriously limits the development and application of low-melting-point multi-component eutectic alloys. In this paper, the low-melting-point multi-component eutectic alloys composed of Bi, Cd, Sn, Pb, and In elements synthesized by high vacuum induction melting and fundamental data were investigated by scanning electron microscopy (SEM), energy dispersive spectrometry (EDS), X-ray diffraction (XRD), differential scanning calorimetry (DSC), and density analysis instrument. Most of the LMP-MCEAs with complex eutectic morphology structures and XRD diffraction patterns could be explained with the fact that they were three-phase eutectic alloys with mixed growth way. Generally, LMP-MCEAs present an extremely low melting point between 48.3 and 124 degrees C and high density between 8 and 10 g/cm3. Copyright (C) 2017, The editorial office of Journal of Materials Science & Technology. Published by Elsevier Limited.

Pre One:Microstructure and texture evolution in the cryorolled CuZr alloy

Next One:Directly cast bulk eutectic and near-eutectic high entropy alloys with balanced strength and ductility in a wide temperature range