    Comparison between dynamic mechanical properties of dam and sieved concrete under biaxial tension-compression

    点击次数:

    论文类型:期刊论文

    发表时间:2017-02-01

    发表刊物:CONSTRUCTION AND BUILDING MATERIALS

    收录刊物:SCIE、EI、Scopus

    卷号:132

    页面范围:43-50

    ISSN号:0950-0618

    关键字:Dam concrete; Sieved concrete; Biaxial tension-compression; Dynamic strength; Strain rate; Failure criterion

    摘要:A comparative study on the dynamic properties of dam and sieved concrete was conducted based on dynamic biaxial tensile-compressive tests. Specimens were designed to be prismatic shape with a size of 250 x 250 x 400 mm for dam concrete and 150 x 150 x 300 mm for sieved concrete, respectively. Each specimen was biaxially loaded by constant tensile-compressive (T-C) stress ratios (0:-1, 0.05:-1, 0.1:-1, 0.25:-1, 0.5:-1, and co) at the strain rate of 10(-5) s(-1), 10(-4) s(-1), 10(-3)s(-1), and 10(-2) s(-1) by a servo-hydraulic multi-axial testing machine. The failure modes of specimens have been compared under various biaxial T-C loading conditions at each strain rate, thus the fracture surface of sieved concrete specimen is smoother than dam concrete. The dynamic strength of dam concrete is lower than sieved concrete under the same loading condition, and the ratio of them is insensitive to strain rate. The growth rates of dynamic strength for dam concrete is consistent with sieved concrete, Whereas much larger than ordinary concrete. By regression of the test results, the dynamic T-C failure criterions for dam and sieved concrete were proposed after considering the combined effects of strain rate and stress ratio. (C) 2016 Elsevier Ltd. All rights reserved.