Hits:
Indexed by:会议论文
Date of Publication:2016-08-16
Included Journals:EI、CPCI-S、Scopus
Page Number:538-541
Key Words:Non-cyanide electroplating; Au-Sn alloys; high stability; Composition optimization
Abstract:A highly stable non-cyanide electroplating bath which can maintain clear at least one month was developed based on Au(III)-Sn(II) using 5,5-dimetheyl-hydantoin (DMH) and pyrophosphate as complexes. The combination of DMH and pyrophosphate can effectively minimize the difference of the deposition potentials between Au and Sn, making the codeposition of Au-Sn alloys possible. The cyclic voltammetry (CV) curve revealed that the codeposition of Au and Sn occurred at the potential of -790mV with a peak potential of -900mV. Pulsed plating was employed to optimize the morphology and composition of Au-Sn alloy films. The effects of pulse frequency, duty percentsge and peak current density on the morphology and composition of the deposits were investigated. The compact Au-Sn eutectic alloy with Sn content controlled from 10 at. % to 50 at. % can be obtained. The Au-Sn deposits were characterized by the scanning electron microscopic (SEM) and energy-dispersive spectroscopic (EDS) analyses.